The large area of flat injection molded parts results in a large shrinkage. The molecular orientation of large injection molded parts is extremely serious, and the cooling of the mold is not uniform, which makes the shrinkage rate of the injection molded parts in all directions inconsistent, resulting in the deformation and distortion of large, thin, flat injection molded parts. Sometimes there is a support bone on one side of the large plane injection molded part, and the injection molded part must be bent toward the side with the bone at this time.
To completely solve the problem of deformation of large flat injection molded parts is indeed a difficult problem, we have summarized some more effective measures to improve the deformation in production.
1. change the mold into a multi-point entry (usually three plate mold), and it is best to reach more than 4 points for large flat injection molded parts above 24 amps. This can reduce the degree of molecular orientation arrangement and reduce the gap of inconsistent shrinkage in all directions.
2. Properly increase the mold temperature, ABS material is usually kept above 60 ℃ to reduce the cooling rate of the injection molded parts, reduce the temperature difference deformation caused by the transition of cooling while reducing the degree of molecular orientation.
3. The most important thing is to increase the injection or holding pressure, and greatly extend the injection or holding time, so that the size of the injection molded part will increase, reduce its shrinkage, and the degree of deformation will be significantly improved. Therefore, extending the injection or holding time (such as extending 10 to 15 seconds) has become an important tool to solve the deformation problem.
4. If the above three measures fail to achieve the desired effect, the only way to take out of the mold is to set. Because the general use of people is not very good, so a little skill is needed.
To sum up.First of all, the injection molded parts should be taken out of the mold early, then, take advantage of the fact that they are still in the state of several tens of degrees high temperature (should still be very hot, this is very critical), put them on the workbench and use the fixture to set the shape, the key is that the design of the fixture needs to be suitable.
At the same time, we should also consider the rebound degree of the injection molded parts, usually 12 hours after the rebound will stop, and the lower the temperature out of the mold, the greater the rebound amount. As the saying goes, the overkill must be corrected, so the amount of overpressure should be studied during production.
Latest blog posts
Custom molds injection molding
Custom molds injection molding is a manufacturing process that involves creating custom molds to produce plastic parts. Injection molding is a popular technique used in various industries such as...
Plastic injection molding companies
Plastic injection molding is a manufacturing process that involves injecting molten plastic into a mold to create a wide range of plastic products. From car parts to medical devices and household items, plastic injection molding is used to create a variet
PET Preform Injection Moulding Machine
PET preform injection molding is a manufacturing process that is used to create PET (polyethylene terephthalate) preforms that can be later blown into bottles, jars, and other containers. This process...
You may like
Pressure control for two-colour injection moulding processes
Pressure control for two-colour injection moulding processes,The two most important processes in two-colour injection moulding are filling and pressure-holding...
Methods for eliminating surface defects of injection molded products
Visible defects on the surface of injection molded products include dark spots, gloss differences or fogged areas, surface wrinkling, or what is known as orange peel. Usually, these defects occur near...
Six scientific injection molding process optimization steps
1)Viscosity curve,The viscosity curve is made to select a suitable injection speed that will not cause large changes in melt viscosity when there are small fluctuations in each parameter. The fluctuation between each mold should be as small as possible to
Analysis of the factors leading to unsuccessful injection molding of two-color injection molds
Two-color injection mold in the process of use will appear in the form of failure, such as plastic deformation failure, plastic mold fracture, cavity surface wear and corrosion, etc., that cause...