Some plastic parts are swollen or blistered on the back of the metal insert or in particularly thick parts soon after molding and demolding. This is because the plastic not completely cooled and hardened under the action of internal pressure penalty release gas expansion caused.
Solution measures.
1. Effective cooling. Reduce the mold temperature, extend the mold opening time, reduce the material drying and processing temperature.
2、Lower the mold filling speed, reduce the molding cycle, and reduce the flow resistance.
3、Improve the pressure and time of holding pressure.
4、Improve the condition that the wall of the part is too thick or the thickness varies greatly.
Analysis of the causes of vibration pattern of injection molded products
PS and other rigid plastic parts form dense ripples on the surface near the gate, sometimes called shock lines.
The reason is that when the melt viscosity is too large and the mold is filled in the form of stagnant flow, the material at the front end quickly condenses and shrinks when it touches the surface of the cavity, while the molten material later expands the cold material that has shrunk and continues to move forward.
Solution.
(1) improve the barrel temperature, especially the injection nozzle temperature, but also to improve the mold temperature.
(2) improve the injection pressure and speed, so that it can quickly fill the cavity.
(3) Improve the flow channel and gate size to prevent excessive resistance.
(4) The mold exhaust should be good, and a large enough cold material well should be set.
(5) Do not design the parts too thin.
Last: Injection Mold Approval Standards Next: Precision injection molding versus general injection molding
Latest blog posts
Custom molds injection molding
Custom molds injection molding is a manufacturing process that involves creating custom molds to produce plastic parts. Injection molding is a popular technique used in various industries such as...
Plastic injection molding companies
Plastic injection molding is a manufacturing process that involves injecting molten plastic into a mold to create a wide range of plastic products. From car parts to medical devices and household items, plastic injection molding is used to create a variet
PET Preform Injection Moulding Machine
PET preform injection molding is a manufacturing process that is used to create PET (polyethylene terephthalate) preforms that can be later blown into bottles, jars, and other containers. This process...
You may like
In order to have a good injection process, injection speed adjustment is indispensable!
Proportional control of injection speed has been widely adopted by injection molding machine manufacturers. Although computer-controlled injection speed segmentation control systems have existed for a long time, the advantages of such machine settings hav
7 factors to consider for injection molding process
I. Shrinkage rate,Thermoplastic molding shrinkage form and calculation as described earlier, the factors affecting the shrinkage of thermoplastic molding are as follows...
The two-color plastic mold produced shrinkage phenomenon of countermeasures
One of the most headache for people who are not very experienced in the processing of two-color plastic moulds is the shrinkage phenomenon that occurs during the processing of two-color plastic moulds.
Analysis of dimensional instability injection molding defects and elimination methods
Dimensional instability refers to the change in the size of plastic parts between each batch of molded products or between each cavity of molded products produced by each mold under...